Save as PDF from the print dialog, pick Destination: Save as PDF. Dialog didn’t appear?
TS-9016 has a fully cured styrene butadiene rubber binder and a blend of Aramid and cellulose fibers.
Specification Properties
| Property | Value | Method |
|---|---|---|
| Density, g/cc(lb/cu.ft) | 1.44 (90) (min.) | ASTM F 1315 |
| Compressibility, % (at 34.5MPa) | 10 - 25 | ASTM F 36 |
| Recovery, % | 40 (min.) | ASTM F 36 |
| Tensile Strength, AMD, MPa(psi) | 12.41 (1800) (min.) | ASTM F 152 |
| Fluid Resistance, IRM903 Oil | ASTM F 146 | |
| Change in Thickness, % | 25 - 65 | |
| Fluid Resistance, Fuel B | ASTM F 146 | |
| Change in Thickness, % | 10 - 40 | |
| Binder Type | Fully Cured Styrene Butadiene |
Test data: Interface Performance Materials, Inc. Values are manufacturer-published specification limits, not field-typical performance. Specific application suitability requires independent evaluation. The supplier’s standard warranty disclaimers apply.